7055 aluminium alloy explained

7055 alloy is heat treatable wrought aluminum alloy.[1] It has high ultimate tensile strength value of 593 MPa.

Chemical Composition

ElementContent (%)
Aluminum85.9 - 88.5
Zinc7.6 - 8.4
Magnesium1.8 - 2.3
Copper2 - 2.6
Iron≤ 0.15
Zirconium0.080 - 0.25
Manganese≤ 0.050
Chromium≤ 0.040
Silicon≤ 0.10
Titanium≤ 0.060
Other (each)≤ 0.050
Other (total)≤ 0.15

Properties

PropertiesSI Unit
Density2.86 g/cm3
Ultimate Tensile Strength[2] 593 MPa
Elongation at Break9.0% to 12.0%
Fracture Toughness24.2 MPa-m½

Applications

  1. Aerospace sector
  2. High strength requirement areas

External links

  1. Single-aging characteristics of 7055 aluminum alloy
  2. 7055: High-Strength Plate and Extrusion Alloy
  3. Microstructure characterization of 7055-T6, 6061-T6511 and 7A52-T6 Al alloys subjected to ballistic impact against heavy tungsten alloy projectile
  4. Grain size prediction and investigation of 7055 aluminum alloy inoculated by Al–5Ti–1B master alloy,Journal of Alloys and Compounds - X-MOL
  5. ShieldSquare Captcha

Notes and References

  1. Web site: 9 May 2013. Aluminium / Aluminum 7055 Alloy (UNS A97055).
  2. Web site: Aluminum 7055-T77511 Extrusions.